Advanced Search

column
In-situ synthesis of Cop Cu composite coating by laser cladding
HE Yizhu, LU Yun
2008(3): 1-4.
[Abstract] [PDF]
Development of wear resisting surfacing electrode with high efficiency, high hardness and low cost
ZHANG Qinghui, XIAO Yifeng, GONG Jianxun
2008(3): 5-8.
[Abstract] [PDF]
Study on PWHT improving toughness at IRCGHAZ of WB36 steel
WANG Xue, CHANG Jianwei, CHEN Fangyu, QIU Minglin
2008(3): 9-12.
[Abstract] [PDF]
Metal magnetic memory signal recognition by neural network for welding crack
DI Xinjie, LI Wushen, BAI Shiwu, LIU Fangming
2008(3): 13-16.
[Abstract] [PDF]
Grain refinement of heat affected zone of high strength low alloy steel by large heat input welding
YU Shengfu, YANG Ke, LEI Yi, YANG Hua
2008(3): 17-20.
[Abstract] [PDF]
Effects of pulsing parameters on weld shape parameters during pulsed Nd-YAG laser welding of aluminum alloys
ZHANG Jing, SHAN Jiguo, LEI Xiang, TAN Wenda, CHEN Wuzhu
2008(3): 21-24.
[Abstract] [PDF]
Toughness mechanism of CGHAZ of 07MnNiCrMoVDR steel
BAI Shiwu, LI Wushen, DI Xinjie, WU Qiang
2008(3): 25-28.
[Abstract] [PDF]
Prediction of performance of heat affected zone and optimization on welding parameters of 07MnNiCrMoVDR steel
ZHANG Jianjun, LI Wushen, DI Xinjie, WU Qiang
2008(3): 29-32.
[Abstract] [PDF]
Slag detachability of new slag system basic electrode
MENG Gongge, YANG Tuoyu, LIU Xiaojing, YANG Lijuan
2008(3): 33-36.
[Abstract] [PDF]
Low temperature toughness of ultra low-carbon 9Ni steel welded joints
WANG Guoping, CHEN Xuedong, WANG Bing
2008(3): 37-40.
[Abstract] [PDF]
Microstructures and mechanical properties of joints of microalloyed EH40 ship steel plate with high heat-input welding
SUN Zhan, HUANG Jihua, ZHANG Hua, ZHAO Xingke, LI Ququan
2008(3): 41-44.
[Abstract] [PDF]
Acicular ferrite microstructure of weld metal for low-alloy steel
HUANG Anguo, YU Shengfu, XIE Mingli, LI Zhiyuan, ZHANG Guodong
2008(3): 45-48.
[Abstract] [PDF]
Review of 9% Ni steel and its weldability
YAN Chunyan, LI Wushen, XUE Zhenkui, BAI Shiwu, FENG Bin
2008(3): 49-52.
[Abstract] [PDF]
Brazing between high purity alumina ceramic and oxygen-free copper
LI Feibin, WU Aiping, ZOU Guisheng, REN Jialie
2008(3): 53-56.
[Abstract] [PDF]
Wettability of two kinds of Pd -Ni brazing filler metals on Si3N4 ceramic
Chen Bo, XIONG Huaping, MAO Wei, LI Xiaohong
2008(3): 57-60.
[Abstract] [PDF]
Dynamic simulation of isothermal solidification in steel Cu steel system rolling-diffusion bonding process
LI Hong, LI Zhuoxin
2008(3): 61-64.
[Abstract] [PDF]
Effect of alloying elements on microstructure and property of AgCuZnSn brazing alloy
LI Zhuoran, JIAO Ning, FENG Jicai, LU Chenghong
2008(3): 65-68.
[Abstract] [PDF]
Fiber bragg grating sensor metallization and embedding into 42CrMo steel by soldering
LI Yulong, FENG Yan, ZHANG Hua, PENG Gang
2008(3): 69-72.
[Abstract] [PDF]
Interface character of high-strength graphite and copper joints brazed with Ti-based amorphous filler metal
XIE Fengchun, HE Peng, FENG Jicai
2008(3): 73-76.
[Abstract] [PDF]
Microstructure and strength of aluminum and aluminum alloy joint brazed with rapidly-cooled Al -Si -Cu-Zn filler metals
ZOU Jiasheng, LV Sicong, ZHAO Hongquan, LUO Xinfeng
2008(3): 77-80.
[Abstract] [PDF]
Effects of 1.0% Zn or Ni additions on interfacial reaction and growth of intermetallics in Sn-3.5Ag Cu joint
YU Chun, XIAO Junyan, LU Hao
2008(3): 81-83.
[Abstract] [PDF]
Stress intensity factor of interfacial crack between metal-base ceramic coating and steel
XU Lianyong, JING Hongyang
2008(3): 84-88.
[Abstract] [PDF]
Microstructure and strength analysis of IC10 alloy TLP-DB joint
HOU Jinbao, ZHANG Lei, WEI Youhui
2008(3): 89-92.
[Abstract] [PDF]
Analysis of characteristic zones of isothermal superplastic welded joint of heterogeneous steels
ZHANG Keke, SHI Hongxin, YU Hua, YANG Yunlin
2008(3): 93-96.
[Abstract] [PDF]
Vacuum hot roll bonding of TC4 titanium alloy and 0Cr18Ni10Ti stainless steel
ZHAO Dongsheng, YAN Jiuchun, YANG Shiqin
2008(3): 97-100.
[Abstract] [PDF]
Influence of creep strength of weld on interfacical creep damage of welded joint of martensitic heat-resistant steel and bainitic heat-resistant steel
ZHANG Jianqiang, HE Jie, ZHANG Guodong, ZHANG Yinglin
2008(3): 101-104.
[Abstract] [PDF]
Finite element simulation of Satoh test taking into account transformation induced plasticity
LIU Junyan, LU Hao, CHEN Junmei, LIU Jinyang
2008(3): 105-108.
[Abstract] [PDF]
Stress-strain around an indentation in measuring residual stress by indentation-strain method
MENG Xianlu, CHEN Huaining, LIN Quanhong, CHEN Jing
2008(3): 109-112.
[Abstract] [PDF]
DC-LSND welding technique of 1420 Al-Li alloy
LIU Ying, GUO Delun, SI Haoxue
2008(3): 113-116.
[Abstract] [PDF]
Fatigue properties of welded joints of 16Mn steel in super long life region
WU Liangchen, WANG Dongpo, DENG Caiyan, WANG Kang
2008(3): 117-120.
[Abstract] [PDF]
Effect of simulated welding parameters on pipe girth weld residual stresses
DONG Junhui, LIN Yan
2008(3): 121-124.
[Abstract] [PDF]
Effect of heated region on stress relief ratio of local heat treatment on spherical tanks
WANG Zejun, LU Huiping, JING Hongyang
2008(3): 125-128.
[Abstract] [PDF]
Calculation and discussion of welding stress and strain field
FANG Hongyuan, ZHANG Xueqiu, YANG Jiangguo, LIU Xuesong
2008(3): 129-132.
[Abstract] [PDF]
Data fusion of multi-sensor in container NC welding machine
CHEN Lihua, TIAN Songya, ZHANG Genyuan, SHI Rusheng, ZHU Xiaohua
2008(3): 133-136.
[Abstract] [PDF]
Microplasma arc sprayed hydroxyapatite coatings
ZHAO Qiuying, HE Dingyong, LI Xiaoyan, LI Zhuoxin, JIANG Jianmin
2008(3): 137-140.
[Abstract] [PDF]
Automatic underwater arc welding seam-tracking system based on flux-core wire and rotating arc sensor
YE Jianxiong, ZHANG Hua
2008(3): 141-144.
[Abstract] [PDF]
Microstructures of high chromium cast iron for surfacing
WEI Jianjun, HUANG Zhiquan, YANG Wei
2008(3): 145-148.
[Abstract] [PDF]
Horizontal welding of pulsed submerged arc welding and its application in oil tank manufacturing
GAO Ying, LI Huan, SUN Bo, YANG Zhansheng
2008(3): 149-152.
[Abstract] [PDF]