Study on changing ruler of plasma in laser welding and the quick testing method of blowhole defects——extract method of feature parameters for blowhole defect
SUN Qian, WANG Xuyou, WANG Wei, LI Xiaoyu XU Fujia, LIAO Ying
2016, 37(6): 1-4.
[Abstract] [PDF]
Microwelding of fused silica by femtosecond laser and the joint mechanical properties
PAN Zehao, CHENG Zhan, LIU Lei, ZOU Guisheng, ZHOU Yunhong
2016, 37(6): 5-8.
[Abstract] [PDF]
Process optimization of laser reflection-induced superimposition deep-penetration welding for titanium alloy sheet
CHENG Man, WANG Hongyu, ZHOU Jianzhong, Li Xiangfeng, HUANG Shu
2016, 37(6): 9-12.
[Abstract] [PDF]
Process stability analysis of double beam laser welding of aluminum alloy
YANG Haifeng, WANG Xuyou, WANG Wei, ZHANG Fu
2016, 37(6): 13-18.
[Abstract] [PDF]
Discrete modeling and deadbeat control of inverter welding power supply
ZHU Zhiming, YANG Zhongyu, TANG Yingying, XIA Zhuliang
2016, 37(6): 19-22,64.
[Abstract] [PDF]
Effect of peak temperature on formation of 6061Al/AZ31BMg dissimilar FSW joint
LIU Zhenlei, CUI Hutao, JI Shude, XU Minqiang, MENG Xiangchen
2016, 37(6): 23-26.
[Abstract] [PDF]
Deformation and failure behavior of friction stir weld joint of 7075 aluminum alloy
CUI Shaopeng, ZHU Hao, GUO Zhu, ZHAO Yipeng
2016, 37(6): 27-30.
[Abstract] [PDF]
Analysis of deviations from local thermal equilibrium in thermal spray plasma jet generated by a DC torch
SUN Chengqi, AN Liantong, YANG Deming, GAO Yang
2016, 37(6): 31-34.
[Abstract] [PDF]
Characteristics of droplet transfer during ultrasound-MIG hybrid welding of aluminum alloy
FAN Chenglei, YAO Qingtai, YANG Chunli, LIN Sanbao, KOU Yi
2016, 37(6): 35-39.
[Abstract] [PDF]
Influence of high energy shot peening on microstructure and properties of TC4 welded joints
HE Xiaomei, WANG Yaomian, ZHANG Conghui
2016, 37(6): 40-44.
[Abstract] [PDF]
Toughness mechanism analysis of submerged arc welding joints of ultra-low carbon bainitic steel
ZHANG Min, CHEN Yangyang, LIU Mingzhi, LI Jihong
2016, 37(6): 45-49.
[Abstract] [PDF]
Fatigue properties and failure mechanisms of self-piercing riveted joints in aluminium alloy
XING Baoying, HE Xiaocong, WANG Yuqi, LIU Fulong
2016, 37(6): 50-54.
[Abstract] [PDF]
Direct laser fusion bonding process of borosilicate glass and Kovar alloy
TIE Min, LI Hong, LI Zhuoxin, JIA Lin
2016, 37(6): 55-58,74.
[Abstract] [PDF]
On-line monitoring and process control of X65 steel pipeline flash butt welding
GAO Shiyi, SHENG An, GUO Chunfu, ZHANG xin
2016, 37(6): 59-64.
[Abstract] [PDF]
Study of intergranular corrosion resistance of overlay by Electroslag cladding with austenitic stainless steel
BAO Yefeng, REN Qiang, ZHANG Zhixi, YANG Ke, JIANG Yongfeng
2016, 37(6): 65-68,79.
[Abstract] [PDF]
Numerical simulation on effect of outer layer gas flow rate and coupling degree on arc characteristics of GPCA-TIG welding
HUANG Yong, LU Suzhong, WANG Xinxin, LI Hui
2016, 37(6): 69-74.
[Abstract] [PDF]
Underwater friction taper plug welding process and mechanical properties of joints for DH36 steel
CUI Lei, YANG Xinqi, WANG Dongpo, CAO Jun
2016, 37(6): 75-79.
[Abstract] [PDF]
Microstructure and mechanical property of A7N01 aluminum alloy welded by laser-MIG hybrid method with assisting ultrasonic vibration
ZHU Zongtao, ZHU Quanchao, LI Yuanxing, CHEN Hui
2016, 37(6): 80-84.
[Abstract] [PDF]
Optimization of GTAW cladding process of Inconel 625 on carbon steel using response surface methodology
LIANG Enbao, HU Shengsun, WANG Zhijiang
2016, 37(6): 85-88,108.
[Abstract] [PDF]
Microstructure and wear-resistance of NiCrBSi coating sprayed-remelted by plasma process
TIAN Lihui, MAO Shuhua, LU Sheng, YAO Zengjian
2016, 37(6): 89-94,113.
[Abstract] [PDF]
EBSD study on microstructure and crystalline orientation of plasma sprayed molybdenum splat
ZHENG Zhenhuan, LI Qiang
2016, 37(6): 95-98.
[Abstract] [PDF]
Narrow gap pulse TIG single-pass one layer welding technology of 508-III steel for nuclear power equipment
FENG Dongxu, GU Wen, AI Danfeng, WANG Xin
2016, 37(6): 99-102.
[Abstract] [PDF]
Effect of residual compressive stress field on fatigue crack growth of B780CF steel welded joints
XUE Bin, ZHANG Tianhui, XU Renping, WANG Shiyue
2016, 37(6): 103-108.
[Abstract] [PDF]
Investigation on one-side welding with back free formation of back weld in horizontal P-TIG
DU Miao, LV Xiaochun, WANG Meng, HE Shi
2016, 37(6): 109-113.
[Abstract] [PDF]
Influence of residual stress on static load strength of under-matching butt joint of high strength steel
ZHAO Zhili, WANG Guanglin, ZHANG Yuanjian, FANG Hongyuan
2016, 37(6): 114-117.
[Abstract] [PDF]
Investigation on sidewall fusion behavior of horizontal narrow gap TIG
WANG Meng, LÜ Xiaochun, LIANG Xiaomei, HE Shi
2016, 37(6): 118-123.
[Abstract] [PDF]
Microstructures of 2219-Al thin-walled parts produced by shaped metal deposition
BAI Jiuyang, FAN Chenglei, YANG Yuchen, XU Yanli, LI Rui, LIN Sanbao, WANG Jihui
2016, 37(6): 124-128.
[Abstract] [PDF]
2016, 37(6): 129-134.