LI Qi, LIU Fengmei, ZHANG Xueyin, YI Yaoyong, GAO Haitao, LI Likun. Effect of Ni-CNTs reinforced particles on the microstructure and mechanical properties of Sn58Bi-0.1Er solder joints[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2021, 42(7): 60-65. DOI: 10.12073/j.hjxb.20201221002
Citation: LI Qi, LIU Fengmei, ZHANG Xueyin, YI Yaoyong, GAO Haitao, LI Likun. Effect of Ni-CNTs reinforced particles on the microstructure and mechanical properties of Sn58Bi-0.1Er solder joints[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2021, 42(7): 60-65. DOI: 10.12073/j.hjxb.20201221002

Effect of Ni-CNTs reinforced particles on the microstructure and mechanical properties of Sn58Bi-0.1Er solder joints

More Information
  • Received Date: December 20, 2020
  • Available Online: August 30, 2021
  • Sn58Bi-0.1Er solder alloys with different Ni-CNTs content were prepared by vacuum melting method, and the effect of different Ni-CNTs content on the wettability of Sn58Bi-0.1Er composite solder on Cu substrate were studied. The interface structure morphology of the intermetallic compound at the joint interface and shear properties under different Ni-CNTs content were analyzed. The results show that when the addition of Ni-CNTs reinforcing particles is 0.01wt% − 0.05wt%, the wettability of the composite solder alloy on the Cu plate is improved, with the further increase of Ni-CNTs content, the wettability of the composite solder on the Cu plate began to show a downward trend. With the addition of Ni-CNTs, the Sn58Bi/Cu interface intermetallic compound transform from serrated Cu6Sn5 to thin layered (Cu, Ni)6Sn5. The addition of Ni-CNTs reinforcing particles can effectively reduce the thickness of the intermetallic compound layer. The addition of Ni-CNTs reinforced particles improves the shear force of the Sn58Bi/Cu joint. When the addition amount of Ni-CNTs is 0.1%, the maximum shear force of the joint is 432.86 N, which is more than twice the shear force of the Sn58Bi-0.1Er solder joint. The addition of Ni-CNTs reinforced particles effectively improves the mechanical properties of the Sn58Bi-0.1Er joint.
  • 李正兵, 胡德安, 陈益平, 等. Fe颗粒对时效过程中SnBi/Cu接头组织及性能影响[J]. 焊接学报, 2020, 41(8): 22 − 28.

    Li Zhengbing, Hu Dean, Chen Yiping, et al. Effect of Fe particles on the structure and properties of SnBi/Cu joint during aging[J]. Transactions of the China Welding Institution, 2020, 41(8): 22 − 28.
    Shen J, Pu Y Y, Yin H G, et al. Effects of minor Cu and Zn additions on the thermal, microstructure and tensile properties of Sn-Bi-based solder alloys[J]. Journal of Alloys and Compounds, 2014, 614(10): 63 − 70.
    Li Y, Chan Y C. Effect of silver (Ag) nanoparticle size on the microstructure and mechanical properties of Sn58Bi-Ag composite solders[J]. Journal of Alloys and Compounds, 2015, 645(5): 566 − 576.
    Suganuma K. Microstructural features of lift-off phenomenon in through-hole circuit soldered by Sn-Bi alloy[J]. Scripta Materialia, 1998, 38(9): 1333 − 1340. doi: 10.1016/S1359-6462(98)00059-1
    Chuang T H, Wu H F. Effects of Ce addition on the microstructure and mechanical properties of Sn-58Bi solder joints[J]. Journal of Electronic Materials, 2011, 40(1): 71 − 77. doi: 10.1007/s11664-010-1385-z
    邱希亮, 郝成丽, 修子扬, 等. 石墨烯纳米片对Sn-58Bi钎料显微组织和性能的影响[J]. 焊接学报, 2017, 38 (4): 63 − 66, 71.

    Qiu Xiliang, Hao Chengli, Xiu Ziyang, et al. Effect of graphene nanoplates on microstructure and properties of Sn-58Bi solders[J]. Transactions of the China Welding Institution, 2017, 38 (4): 63 − 66, 71.
    Yang L, Du C C, Dai J, et al. Effect of nanosized graphite on properties of Sn-Bi solder[J]. Journal of Materials Science: Materials in Electronics, 2013, 24(11): 4180 − 4185. doi: 10.1007/s10854-013-1380-2
    Li Q, Wu H, Xiong M, et al. Effect of Er on microstructure and mechanical properties of Sn58Bi based lead-free solder[C]//2020 International Conference on Artificial Intelligence and Electromechanical Automation (AIEA). IEEE, Tianjin, China, 2020: 648-653.
    Li Q, Xiong M, Liu F, et al. Effect of Er content on the interfacial microstructure, shear properties and creep properties of Sn58Bi joints[J]. IOP Conference Series: Earth and Environmental Science, 2021, 714(3): 032017. doi: 10.1088/1755-1315/714/3/032017
    Gain A K, Zhang L. Growth mechanism of intermetallic compound and mechanical properties of nickel (Ni) nanoparticle doped low melting temperature tin-bismuth (Sn-Bi) solder[J]. Journal of Materials Science Materials in Electronics, 2016, 27: 781 − 794. doi: 10.1007/s10854-015-3817-2
    杨立壮. 镍、镀镍碳纳米管增强 Sn58Bi 无铅焊料微观结构与机械性能的研究[D]. 天津: 天津大学, 2014.

    Yang Lizhuang. Microstructure and mechanical properties of Ni and Ni-coated carbon nanotubes reinforced Sn58Bi lead-free solder[D]. Tianjin: Tianjin University, 2014.
    王春青, 李明雨, 田艳红, 等. JIS Z 3198 无铅钎料试验方法简介与评述[J]. 电子工艺技术, 2004, 25(2): 47 − 54. doi: 10.3969/j.issn.1001-3474.2004.02.001

    Wang Chunqing, Li Mingyu, Tian Yanhong, et al. Review JIS Z 3198: Test Method for Lead-free Solder[J]. Electronic Process Technology, 2004, 25(2): 47 − 54. doi: 10.3969/j.issn.1001-3474.2004.02.001
    Yang L, Wei Z, Li X, et al. Effect of Ni and Ni-coated carbon nanotubes on the interfacial reaction and growth behavior of Sn58Bi/Cu intermetallic compound layers[J]. Journal of Materials Science Materials in Electronics, 2016, 27(11): 1 − 7.
    Qi L, Gao H, Xiong M, et al. Effect of Ni-CNTs on microstructure, thermodynamic characteristic and mechanical properties of Sn58Bi-0.1 Er based lead-free solder[C]//2020 21st International Conference on Electronic Packaging Technology (ICEPT). IEEE, Guangzhou, China, 2020: 1-6.
  • Related Articles

    [1]WU Kaiyuan, HE Zuwei, LIANG Zhuoyong, HUANG Xi. Double pulse welding method for twin-wire pulsed MIG welding[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2017, 38(5): 53-57. DOI: 10.12073/j.hjxb.20170512
    [2]WU Kaiyuan, ZHANG Tao, HE Zuwei, LI Huajia. STM32 based power supply system for integrative twin-wire pulsed MIG welding[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2015, 36(11): 25-28.
    [3]LÜ Yan, TIAN Xincheng, LIANG Jun. Decoupling control design and simulation of aluminum alloy pulsed MIG welding based on dynamic PLS framework[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2013, (6): 17-20.
    [4]LU Lihui, FAN Ding, HUANG Jiankang, ZHU Ming, SHI Yu. Study on arc length control system for pulsed MIG welding of aluminum alloy[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2011, (9): 53-56.
    [5]LU Lihui, SHI Yu, HUANG Jiankang, FAN Jiawei, FAN Ding. Vision sensing and control for wire extension in pulsed MIG welding of aluminum alloy[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2011, (7): 63-66.
    [6]HUANG Jiankang, SHI Yu, LU Lihui, ZHU Ming, FAN Ding. Weld width control of double pulsed MIG welding for aluminum alloy[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2011, (5): 13-16.
    [7]SHA Deshang, Liao Xiaozhong. Full digital control of I/I mode pulsed MIG welding based on triple closed loop control[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2009, (4): 5-7,12.
    [8]PENG Haiyan, HUANG Shisheng, WU Kaiyuan, WANG Zhenmin. Digital control system based on DSP for pulsed MIG welding[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2008, (9): 63-66.
    [9]SHI Yu, XUE Cheng, FAN Ding, LI Jianjun. Modeling and simulation of decoupling control system of aluminum pulsed MIG welding[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2008, (5): 9-12.
    [10]YANG Li-jun, LI Huan, HU Sheng-gang, LI Jun-yue. Pulsed MIG Welding Inverter Power Source by Spectral and Control System[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2001, (1): 41-44.

Catalog

    Article views (502) PDF downloads (25) Cited by()

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return