Advanced Search
WANG Jian, WEI Shanchun, LIN Tao, CHEN Shanben. Application of image morphology in detection of initial welding position[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2012, (4): 21-24.
Citation: WANG Jian, WEI Shanchun, LIN Tao, CHEN Shanben. Application of image morphology in detection of initial welding position[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2012, (4): 21-24.

Application of image morphology in detection of initial welding position

More Information
  • Received Date: February 27, 2011
  • The image morphology was introduced to detect the initial welding position of straight welding seam.The straight seam image was acquired by using a small CCD camera.The erosion edge detection algorithm was used to process the image,which could maintain the key information and eliminate other interference.Finally the initial welding position was obtained by filter with directional liner structure elements and Hough transformation.The whole processing is very intuitionistic,simple and fast.In addition,it's higher self-adaptability,higher process accuracy and stronger robustness.This research can meet the need of practical work,and lay a good foundation for the guidance of initial welding position.
  • Related Articles

    [1]YANG Wenyan, FAN Ding, ZHANG Junxi. Formation mechanism and influencing factors of unstable metal transfer in high current MAG welding[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2023, 44(11): 110-116. DOI: 10.12073/j.hjxb.20230131001
    [2]ZOU Li, REN Siyuan, YANG Guang, YANG Xinhua. Analysis of factors affecting fatigue life of welded joints based on improved conditional neighborhood entropy[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2021, 42(11): 43-50. DOI: 10.12073/j.hjxb.20210323001
    [3]YANG Xinhua, JIA Xin, ZHU Ping, LI He. Analysis of factors affecting fatigue performance of welded joints based on information gain rate[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2020, 41(10): 73-78. DOI: 10.12073/j.hjxb.20200808001
    [4]CUI Haipo, LIU Xiaojie, DENG Deng. Influence factors for electromigration of metal interconnects[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2018, 39(5): 29-32. DOI: 10.12073/j.hjxb.2018380116
    [5]FANG Xifeng, WANG Xin, SHI Xuehai, JI Shude, LIANG Zhimin, XIAO Hanlin. Effects of temperature on microstructure and fracture position of MIG welded joints using circled wire-feeding mode[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2016, 37(12): 37-40.
    [6]XUE Peng, XUE Songbai, SHEN Yifu, LONG Weimin, ZHANG Qingke, MA Jia. Effect of temperature and coatings on the wettability of Sn- Zn-Ga-Nd lead-free solder[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2013, (8): 31-34.
    [7]WANG Jing, LU Minxu, YANG Ping, ZHANG Lei, CHANG Wei. Effect of temperature on CO_2 corrosion of dissimilar weld joint[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2012, (11): 26-30.
    [8]ZHAO Huaxia, JIAO Xiangdong. Welding arc temperature in hyperbaric TIG welding[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2008, (11): 17-20.
    [9]Sun Xian, Bai Yingbin, Liu Mingliang, et al. Research on Droplet Transfer and Its Influence Factors of Stainless Steel Electrode[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2000, (1): 25-29.
    [10]Yin Yousheng. Brittleness of Brazed Seam for Nickel-base Brazing Filler Metals and Its Influnce Factors[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 1997, (3): 134-140.

Catalog

    Article views (234) PDF downloads (90) Cited by()

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return