Gray scale morphological analysis on molten pool image of metal active-gas welding

More Information
  • Received Date: September 21, 2005
  • In the welding process,the method of image processing has been getting more and more important,especially in tracking control and quality molding.The mathematical morphology is used to analyze the MAG(metal active-gas) welding images.In addition to using the four fundamental gray-scale morphological operations,we especially design a set of the gray-scale morphological algorithms from the image preprocessing to the edge detection on the MAG welding image.The experiment results illustrated that the chosen algorithms were very suitable to the image processing of the welding molten pool.
  • Related Articles

    [1]JIANG Wenchun, GU Wenbin, JIN Qiang, WANG Jinguang, WU Aibing, TU Shandong. Local post weld heat treatment method by primary and secondary distributed heat source[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2023, 44(5): 27-35. DOI: 10.12073/j.hjxb.20220608002
    [2]ZHANG Yuelai, PENG Zhangzhu, CHANG Maochun, HU Long, PAN Guochang, XU Bo. Numerical simulation of residual stress in complex aluminum alloy welded structure[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2021, 42(3): 91-96. DOI: 10.12073/j.hjxb.20201215001
    [3]LÜ Yishi, JING Hongyang, XU Lianyong, HAN Yongdian, LIU Faan. Welding residual stress in T-joint after TIG dressing and its relief[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2012, (9): 37-40.
    [4]GUAN Jianjun, CHEN Huaining. Numerical simulation of relieving residual stresses in medium-thick plate butt-joints by explosive treatment[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2011, (9): 105-108.
    [5]JI Shude, ZHANG Liguo, FANG Hongyuan, LIU Xuesong. Analysis on runner welding residual stress affected by local heating[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2007, (4): 97-100.
    [6]JI Shude, ZHANG Liguo, FANG Hongyuan, LIU Xue-song. Influence of local heating-cooling on welding residual stress of francis turbine runner[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2007, (2): 71-74.
    [7]HOU Hai-liang, ZHU Xi, LIU Run-quan. Welding residual stress relieving of steel 921A of using explosive method[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2004, (1): 119-123.
    [8]Zhu Zheng-qiang, Ge Jing-guo, Rao De-ling, Chen Li-gong. Investigation on vibration stress relief of post-welded drums[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2003, (6): 66-68.
    [9]WANG Zhe-chang. Discuss on Principle of Relieving Welding Residual Stress[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2000, (2): 55-58.
    [10]Cai jie, Wang Yuanliang, Chen Mingming. Measurement of residual stress in big weldment and vibraticn stress relieving[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 1991, (2): 89-95.

Catalog

    Article views (307) PDF downloads (60) Cited by()

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return