Advanced Search
LIU Quanming, LONG Weimin, FU Li, ZHONG Sujuan, LI Xiupeng. Tensile properties evolution of hydrogen-induced TA10 titanium alloy welded joints[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2020, 41(12): 20-24. DOI: 10.12073/j.hjxb.20200615003
Citation: LIU Quanming, LONG Weimin, FU Li, ZHONG Sujuan, LI Xiupeng. Tensile properties evolution of hydrogen-induced TA10 titanium alloy welded joints[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2020, 41(12): 20-24. DOI: 10.12073/j.hjxb.20200615003

Tensile properties evolution of hydrogen-induced TA10 titanium alloy welded joints

More Information
  • Received Date: June 14, 2020
  • Available Online: January 07, 2021
  • Hydrogen embrittlement of titanium alloy weldments often occur at low hydrogen concentrations. The effect of hydrogen content on tensile properties of titanium alloy welded joints and its mechanism were studied. The results show that with the increase of hydrogen content, the room temperature strength was significantly improved, the plasticity was significantly deteriorated. At 0.05 wt.% H, solid solution hydrogen had a limited effect on tissue strengthening and a slight increase in tensile strength; solid solution hydrogen reduced the "pinning" effect of solute atom on dislocation movement, yield strength decreased; solid solution hydrogen only depend on the diffusion and accumulation to cause the local micro-region hydrogen concentration to increase, which had a little effect on the plasticity. After 0.12 wt.% H, the "pinning" effect of the hydride was strengthened, the hydrogen-induced dislocation cross-slip was more difficult, and the strength at room temperature was significantly increased; the brittle hydride itself fractured, precipitated, or accelerated separation from the matrix, resulting in significant plasticity decline. When not charged with hydrogen or 0.05 wt.% H, the ductile fracture occurred in the welded joint; After 0.12 wt.% H, the brittle fracture was the main; solid solution hydrogen and the hydride had a direct effect on fracture mode transformation.
  • 张春波, 乌彦全, 朴东光, 等. TA19钛合金惯性摩擦焊接工艺[J]. 焊接学报, 2018, 39(12): 44 − 48. doi: 10.12073/j.hjxb.2018390295

    Zhang Chunbo, Wu Yanquan, Piao Dongguang, et al. TA19 titanium alloy inertia friction welding process[J]. Transactions of the China Welding Institution, 2018, 39(12): 44 − 48. doi: 10.12073/j.hjxb.2018390295
    Qi Dan, Zhu Ying, Guo Wei, et al. New Ti-Zr-Cu-Ni-La system brazing filler metals for the joining of titanium alloy[J]. China Welding, 2015, 24(2): 6 − 11.
    Li Xifeng, Chen Xin, Li Baoyong, et al. Grain refinement mechanism of Ti-55 titanium alloy by hydrogenation and dehydrogenation treatment[J]. Materials Characterization, 2019, 157: 109919. doi: 10.1016/j.matchar.2019.109919
    Panin P V, Manokhin S S, Dzunovich D A. Research on submicron-grained structure formation in titanium alloys upon reversible hydrogenation and plastic deformation[J]. Inorganic Materials Applied Research, 2018, 9(6): 1029 − 1034. doi: 10.1134/S2075113318060229
    中国国家标准化管理委员会. GB/T 2651-2008 焊接接头拉伸试验方法[S]. 北京: 中国标准出版社, 2008.

    Standardization Administration of the People’s Republic of China. GB/T 2651-2008 Tensile test method on welded joints[S]. Beijing: Standards Press of China, 2008.
    Liu Quanming, Zhang Zhaohui, Yang Haiying, et al. Hydride precipitation in the hydrogenated 0.12wt.%H weld zone of Ti-0.3Mo-0.8Ni alloy argon-arc-welded joints[J]. The Journal of the Minerals, Metals & Materials Society, 2018, 70(9): 1902 − 1907.
    Liu Quanming, Zhang Zhaohui, Liu Shifeng, et al. The hydride precipitation mechanisms in the hydrogenated weld zone of Ti-0.3Mo-0.8Ni alloy argon-arc welded joints[J]. Advanced Engineering Materials, 2018, 20(5): 1700679. doi: 10.1002/adem.201700679
    褚武扬. 氢损伤和滞后断裂[M]. 北京: 冶金工业出版社, 1988.

    Chu Wuyang. Hydrogen damage and delayed fracture[M]. Beijing: Metallurgical Industry Press, 1988.
    苏娟华, 邵鹏, 任凤章. TA10钛合金高温流变行为及拉伸性能[J]. 材料热处理学报, 2018, 39(6): 14 − 20.

    Su Juanhua, Shao Peng, Ren Fengzhang. High temperature flow behavior and tensile properties of TA10 titanium alloy[J]. Transactions of Materials and Heat Treatment, 2018, 39(6): 14 − 20.
    施金美. 钛合金环境氢脆的研究[D]. 上海: 上海大学, 2003.

    Shi Jinmei. Study on environmental hydrogen embrittlement of titanium alloy[D]. Shanghai: Shanghai University, 2003.
    Anand L, Mao Y, Talamini B. On modeling fracture of ferritic steels due to hydrogen embrittlement[J]. Journal of the Mechanics and Physics of Solids, 2019, 122: 280 − 314. doi: 10.1016/j.jmps.2018.09.012
    袁宝国. 置氢Ti-6Al-4V合金室温变形行为及改性机理研究[D]. 哈尔滨: 哈尔滨工业大学, 2010.

    Yuan Baoguo. Deformation behavior and mechanism of hydrogenated Ti-6Al-4V alloy at room temperature[D]. Harbin: Harbin Institute of Technology, 2010.
  • Related Articles

    [1]CHI Luxin, GU Lingxiang, XU Huibin, HUANG Yan, QIN Quan, RAN Yang. Corrosion behavior of joints by electromagnetic pulse welding with aluminum to steel in neutral salt spray[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2023, 44(2): 40-47. DOI: 10.12073/j.hjxb.20220909003
    [2]JIAO Shuaijie, WANG Guofu, JIA Yuli, LI Xiangyang, YANG Yuting, HAN Ying. Impact performance optimization of supermartensitic stainless steel welding wire deposited metal by MAG welding[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2022, 43(3): 93-100. DOI: 10.12073/j.hjxb.20210920002
    [3]FANG Weiping, XIAO Tie, ZHANG Yupeng, Xu Wanghui, YI Yaoyong. Stress corrosion crack sensitivity of ultra-thick TC4 titanium alloy electron beam welding joints[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2019, 40(12): 121-128. DOI: 10.12073/j.hjxb.2019400324
    [4]ZHANG Qunbing, NIU Jing, ZHAO Pengfei, HUANG Yong, LI Zhigang, ZHANG Jianxun. Influence of preheating temperature on cold cracking sensitivity of 12Cr10Co3W2Mo heat resistant steel[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2015, 36(4): 87-91.
    [5]LI Xiaoquan, CHU Yajie, YANG Zonghui, HE Xiancong. Effect of hot extrusion deformation on microstructure and fracture morphology of AZ31B magnesium alloy TIG weld seam[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2012, (3): 1-4.
    [6]WU Huibin, LIANG Guoli, TANG Di. Effects on mechanical properties of high welding heat-input for EH36 shipbuilding steel joint[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2012, (2): 57-60.
    [7]LI Liying, WANG Yong, LI Hongwei, HAN Tao, LI Chaowen. Microstructure and toughness in reheated CGHAZ of ASTM4130 steel[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2011, (6): 33-36.
    [8]ZHANG Liang, XUE Songbai, HAN Zongjie, YU Shenglin, SHENG Zhong. Investigation of mechanical property and fracture morphology of lead-free soldered joints of fine pitch devices[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2008, (9): 35-38.
    [9]Dong Junhui, Yao Jun, Li Jianguo, et al. Microstructure and Mechanical Properties in Welded Joint of High Purity Cr30Mo2 Ferritic Stainless Steel[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2000, (1): 94-96.
    [10]Yang Shijie, Meng Qingsen, Lu Wenxiong. Fracture morphology of solidification crack and crack resisting property of austenitic stainless steel deposited metal[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 1995, (2): 62-67.

Catalog

    Article views (447) PDF downloads (29) Cited by()

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return