Research on Technology of Detecting Welding Seam Based on Gauss Wavelet

More Information
  • Received Date: January 06, 2002
  • Based on the technology of edge detection by wavelet transform,a new method of detecting seam of welding pipe using Gauss wavelet is proposed.As Gauss wavelet has local characteristics on the time and frequency domain,it is suitably used to detect the local shape of a signal as welding seam.The paper mainly relates to the pretreatment of the seam image,the Gauss wavelet transform and its application on the detecting welding seam,and the correlation analysis on the ultimate results.The scale parameter has outstanding effects on the transform results.By the analysis and the simulation on computer,the method shows higher estimated precision and better capability of anti disturb.In the other hand,its complication is not high.So it can be used into real time control system.
  • Related Articles

    [1]JING Hongyang, SHANG Jin, XU Lianyong, HAN Yongdian. Corrosion failure analysis for heat exchanger[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2016, 37(9): 1-4.
    [2]SUN Ji, GUI Chibin, CHEN Wenjun. Safety assessment for under-matched joints of 10CrNi3MoV steel with different values of weld toughness[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2012, (2): 69-72.
    [3]DENG Caiyan, ZHANG Yufeng, HUO Lixing, WANG Dongpo, LUO Hong. Analysis on leak-before-break safety assessment of pressurized pipes[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2008, (4): 25-28.
    [4]XU Zunping, CHENG Nanpu, LEI Binlong, CHEN Zhiqian. Safety assessment of surface pit in penstock[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2007, (8): 62-64.
    [5]ZHANG Manli, WANG Jianping, TAO Yongyin. Ductile tearing assessment of surface flaw in circumferential weld of pipe-line based on J integral parameter[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2007, (2): 59-62.
    [6]LIU Ming-liang, ZHANG Yu-feng, HUO Li-xing, DENG Cai-yan. Safe assessment for overmatching welded joint of offshore pipeline[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2006, (5): 31-34.
    [7]XIA Jing, HUO Li-xing, BAI Bing-ren, CAO Jun. Safe assessment of surface flaw under mismatched weld in offshore pipeline[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2005, (9): 39-43.
    [8]ZHANG Min, MA Bo. Failure assessment curves of double-parameter J-Q criterion of welded joints containing defect(Ⅱ)[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2004, (6): 38-42.
    [9]DENG Cai-yan, ZHANG Yu-feng, HUO Li-xing, ZHANG Li, BAI Bing-ren, LI Xiao-wei, CAO Jun. Safe assessment for welded joint of offshore pipeline[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2004, (6): 27-30,34.
    [10]Zhang Min, Ma Bo. Failure assessment curve of double-parameter J-Q criterion of welded joints containing defects (Ⅰ)[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2004, (5): 93-98.

Catalog

    Article views (202) PDF downloads (51) Cited by()

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return