INFLUENCE OF SMALL AMOUNT OF NICKEL ON THE BRITTLE TRANSITION TEMPERATCURE OF GRANULAR BAINITIC WELDS

  • A small amount (0.12% to 0.36%) of nickel can lower the granular bainite transformation temperature, decrease the average area of M-A constituent in the granular bainite, raise the cleavage fraclure stress of the weld,and hence lower the brittle transition temperature of the weld.