高级检索

石英玻璃/TC4钛合金脉冲串飞秒激光焊接接头组织及性能分析

Microstructure and property analysis of quartz glass/TC4 titanium alloy joints welded by burst-mode femtosecond laser

  • 摘要: 为实现石英玻璃与TC4钛合金的高质量连接,采用脉冲串输出式飞秒激光对二者进行了焊接试验,重点考察脉冲串内所有单个脉冲能量的总和,即脉冲串能量,与一个脉冲串所包含的子脉冲数量,即子脉冲数两种工艺参数对焊接质量的影响.结果表明,脉冲串能量和子脉冲数主要影响激光对材料的局部热输入;热输入过高时,石英玻璃母材中会形成激光影响区,破坏其成分均一性.经工艺优化,确定最佳参数为脉冲串能量300 μJ、子脉冲数4.在此条件下,焊接界面形成连续、致密的熔合层,无气孔及未熔合缺陷,且此时接头抗剪强度最高,为27.2 MPa. EDS与TEM分析表明,Ti,Si及O元素充分互扩散,熔合层内生成TiO2和TiO两种次生相,实现机械-化学混合连接.应力及断口分析进一步表明,过高热输入会加剧母材热膨胀,在界面产生垂直拉应力,甚至诱发石英玻璃内部脆断.

     

    Abstract: Abstract: To achieve high-quality joining between quartz glass and TC4 titanium alloy, welding experiments were conducted on the two materials using a burst-mode femtosecond laser, focusing on the effects of two process parameters on welding quality: the burst energy, i.e., the sum of the energies of all individual pulses within a burst, and the sub-pulse count, i.e., the number of sub-pulses contained in one burst. It was found that these two process parameters primarily affect the local heat input of the laser to the material. When the heat input is excessive, a laser-affected zone forms in the quartz glass base material, destroying its compositional homogeneity. Through process optimization, the optimal parameters were determined as a burst energy of 300 μJ and a sub-pulse count of 4. Under these conditions, a continuous and dense fusion layer was formed at the welding interface, free from pores and lack-of-fusion defects, and the shear strength of the joint reached its maximum of 27.2 MPa. EDS and TEM analyses revealed sufficient interdiffusion of Ti, Si, and O elements, with two secondary phases, TiO2 and TiO, generated within the fusion layer, forming a mechanical-chemical hybrid joint. Stress and fracture analyses further indicate that excessive heat input exacerbates the thermal expansion of the base materials, generating tensile stress perpendicular to the interface and even inducing brittle fracture within the quartz glass.

     

/

返回文章
返回