Effect of travel speed on the root-defects and mechanical properties of friction stir welded A6082 alloy joint

  • 摘要: 研究了不同焊接速度对5.1 mm厚6082-T6铝合金搅拌摩擦焊接头根部缺陷及性能的影响.采用光学显微镜观察了不同参数下接头根部缺陷形貌并对不同焊接速度下的接头进行了拉伸和弯曲试验.结果表明,随着焊接速度的不断增加,接头根部未焊透缺陷倾向变大,接头软化区部位最低硬度值逐渐增高.焊接速度由50 mm/min增大到400 mm/min时,接头抗拉强度逐渐增加.进一步增大焊接速度到600 mm/min时,由于根部未焊透缺陷的严重性变大,造成接头强度下降.在软化区是接头薄弱区的条件下,其尺寸较小的根部缺陷不影响接头抗拉强度.但是对接头的抗弯强度有显著的不利影响.

     

    Abstract: Effect of different travel speeds on the root-defects and mechanical properties of friction stir welded 5.1 mm thick A6082-T6 alloy joint was investigated in this study. The root-defect and microstructure of joints were observed by optical microscope, the tensile and bending tests of joints with different travel speeds were conducted. The results showed that the tendency of incomplete penetration defect and the lowest hardness of softening area in joints were increased with increasing travel speed. The tensile strength of FSW welded A6082-T6 alloys was increased with increasing travel speed from 50 mm/min to 400 mm/min. When travel speed was further increased to 600 mm/min, the tensile strength of joint decreased because of serious incomplete penetration defect. It was found that the small size root-defect had little effect on the tensile property whereas a deleterious effect on bending properties of the friction stir welded A6082-T6 alloy joint.

     

/