  • 摘要: 采用超声疲劳振动技术研究了桥梁钢Q345qC的母材和圆形对接焊接接头试件的高周与超高周疲劳性能.试验发现,在105~109循环周次内焊接接头的疲劳性能远低于母材,且无论是母材还是焊接接头其S-N曲线都是呈连续下降趋势.当母材服役超过107周次,焊接接头服役超过5×106周次以后,试件仍然发生疲劳断裂.结果表明,焊接接头试件断口位置主要位于熔合区的焊趾处或焊接接头表面几何非连续处;在高应力区,疲劳失效多发生于接头表面几何非连续处,在低应力区,疲劳失效多发生于焊趾处.

     

    Abstract: The high cycle and ultra-high cycle fatigue properties of Q345qC base metal and circular butt weld joint were studied by using the ultrasonic fatigue testing technique. The experimental results show that during 105-109 cycles, the fatigue strength of welded joint is much less than that of base metal, and both their S-N curves descend continuously. Fracture can still occur on base metal beyond 107 cycles and on welded steel beyond 5×106 cycles. The observation of fracture surface shows cracks mainly initiate from welded toes at fusion area or geometric discontinuity at the surface in welded steel. Furthermore, fatigue failure occurs at the geometric discontinuity area in the high stress regime but occurs at welded toes in the low stress regime.

     

/