高级检索
韩丽青, 林国标, 王自东, 李锋, 白兴国. 热等静压对钛不锈钢焊接接头组织性能的影响[J]. 焊接学报, 2008, (11): 41-44.
引用本文: 韩丽青, 林国标, 王自东, 李锋, 白兴国. 热等静压对钛不锈钢焊接接头组织性能的影响[J]. 焊接学报, 2008, (11): 41-44.
HAN Liqing, LIN Guobiao, WANG Zidong, LI Feng, BAI Xingguo. Influence of hot isostatic pressing on structure and properties of titanium/stainless steel joint by explosive welding[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2008, (11): 41-44.
Citation: HAN Liqing, LIN Guobiao, WANG Zidong, LI Feng, BAI Xingguo. Influence of hot isostatic pressing on structure and properties of titanium/stainless steel joint by explosive welding[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2008, (11): 41-44.

热等静压对钛不锈钢焊接接头组织性能的影响

Influence of hot isostatic pressing on structure and properties of titanium/stainless steel joint by explosive welding

  • 摘要: TA2/316L爆炸焊接试样在压力150MPa,温度850℃条件下热等静压处理2h,分别对爆炸态和热等静压态焊接接头进行了抗剪强度测试,重点对比研究了热等静压处理对焊接接头组织形貌、化学成分分布及脆性相的影响。热等静压处理后,原爆炸态接头附近的缺陷被治愈,Ti,Cr,Fe,Ni等元素的相互扩散距离明显增加,但接头中生成的脆性相也增加。结果表明,爆炸态的剪切试样断裂于TA2侧,热等静压态断裂于金属间化合物相。

     

    Abstract: TA2/316L joints acquired by explosive welding were treated by hot isostatic pressing treatment at the pressure of 150 MPa and at 850℃ for 2 hours.The effects of the treatment on the shear strengths, microstructure and chemical composition distribution of the joints were investigated.The treatment made the defects in the joints heal and inter-diffusion space of Ti, Cr, Fe and Ni be longer and also the embrittlement phases increase.The treated samples breaks along embrittlement phase during shear tests, which is different from the samples before treatment, and it generally fails at TA2 alloy sides of the joints.

     

/