程江波, 梁秀兵, 陈永雄, 刘燕, 徐滨士, 吴毅雄. 再制造电弧喷涂成形层的残余应力分析[J]. 焊接学报, 2008, (6): 17-20.
引用本文: 程江波, 梁秀兵, 陈永雄, 刘燕, 徐滨士, 吴毅雄. 再制造电弧喷涂成形层的残余应力分析[J]. 焊接学报, 2008, (6): 17-20.
CHENG Jiangbo, LIANG Xiubing, CHEN Yongxiong, LIU Yan, XU Binshi, WU Yixiong. Residual stress in electric arc sprayed coatings for remanufacturing[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2008, (6): 17-20.
Citation: CHENG Jiangbo, LIANG Xiubing, CHEN Yongxiong, LIU Yan, XU Binshi, WU Yixiong. Residual stress in electric arc sprayed coatings for remanufacturing[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2008, (6): 17-20.

再制造电弧喷涂成形层的残余应力分析

Residual stress in electric arc sprayed coatings for remanufacturing

  • 摘要: 阐述了热喷涂涂层中残余应力的产生原因,并利用XRD残余应力测试仪、纳米压痕仪、扫描电镜和X射线衍射仪研究了不同厚度和热处理温度下电弧喷涂7Cr13涂层的残余应力、弹性模量及涂层微观结构。结果表明,涂层的残余应力与厚度成正比关系。适当的热处理工艺能够释放涂层的残余拉应力,当热处理的温度在200~300℃之间时,涂层由拉应力转变为压应力,并随着温度的升高,压应力逐渐增大;涂层的弹性模量和热处理温度之间成正比关系。通过对涂层残余应力分布的研究,为喷涂成形较厚涂层提供了一定的理论依据和方法。

     

    Abstract: The residual stresses in different thickness and different annealing temperatures of electric arc sprayed 7Cr13 coatings were investigated.The microstructure, elastic modulus and residual stress of the coatings were characterized by SEM, XRD, nano-indentation tester and XRD residual stress tester.The results show that the residual stress in the coating is increasing with increasing of the coating thickness.Annealing treatment can release the residual tensile stress of the coatings.When the annealing temperature is between 200-300℃, tensile stress can change from tenstle stress to compress stress in the coatings.The elastic modulus of the coatings is increasing with increasing of annealing temperature.Based on the results mentioned above, some advice and methods to spray forming thickness coatings can be given.

     

/