铝合金平板搅拌摩擦焊接应力变形分析

Residual stress and distortion of Al alloy panels welded by FSW

  • 摘要: 针对6056-T6铝合金平板进行搅拌摩擦焊接和试板变形检测试验。并用数值方法对试板变形进行模拟,考察了模拟温度、应力场分布和试板变形情况,对试验和模拟温度、变形进行比较。结果表明,在文中条件下,沿焊缝长度方向试板产生下挠,最大变形量6.3mm;沿试板宽度方向试板相对发生上拱,最大变形量4.5mm,模拟与实测变形趋势非常吻合。纵向残余应力在焊缝中心线两侧非对称性分布,前进侧大于回转侧。

     

    Abstract: FSW 6056-T6 Al alloy panel was welded by FSW and its distortion was measured.Also numerical model was established to simulate the distortion, temperature field and stress fields. The simulated temperature and distortion were compared with those of experiments.The results indicated that the panel bent down along welding direction and maximum distortion reaches 6.3 mm.Along the transverse direction, the panel bent up relatively to the longitudinal sides and the maximum displacement was 4.5 mm.There were high accordance trends of simulated distortion to the experiment.The longitudinal residual stress was asymmetric with the weld center line and it is higher on advancing side.

     

/