镁合金小孔变极性等离子弧缝焊工艺

Lap seam welding of magnesium alloy with variable polarity plasma arc

  • 摘要: 采用小孔变极性等离子弧缝焊工艺实现了AZ31B镁合金板材的连接,得到了高质量的焊接接头,焊后利用光学显微镜、万能拉伸试验机和显微硬度仪等设备对焊接接头的组织与性能进行了检测分析。结果表明,小孔变极性等离子弧缝焊工艺可以在不开坡口、不需背面强制成形保护的条件下,实现单面施焊双面获得良好的成形;焊接接头的热影响区不明显,平均拉伸剪切力能达到7.3kN以上;焊缝区组织均匀,晶粒细小,硬度值均高于母材;是一种理想的提高镁合金焊接效率和质量的方法。

     

    Abstract: The keyhole variable polarity plasma welding was used to weld AZ31BMg alloy, and favorable joint was obtained.The microstructure, mechanical properties and hardness were investigated by the optical microscope, tensile testing machine and hardness instrument.The results show that one side welding with back formation can be obtained through this technique when there is no groove and no enclosed protection;the heat-affected zone is narrow, and the average tensile shear is 7.3 kN;the grains of fusion zone are fine, and the hardness of welded joint is higher than that of the base metal.In summary, the variable polarity plasma arc welding process is a perfect method to weld Mg alloy, which can improve the microstructure of the joint and increase the welding quality.

     

/