魏琪, 李文静, 朱学军, 胡强. 时效硬化工具合金TIG金属粉芯焊丝堆焊金属硬度和红硬性[J]. 焊接学报, 2002, (3): 49-52.
引用本文: 魏琪, 李文静, 朱学军, 胡强. 时效硬化工具合金TIG金属粉芯焊丝堆焊金属硬度和红硬性[J]. 焊接学报, 2002, (3): 49-52.
WEI Qi, LI Wen-jing, ZHU Xue-jun, HU Qiang. Study on Hardness and Redhardness of Surfacing Metal of Metal Powder-Cored Wire of Age Hardening Tool Alloy for TIG Surfacing[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2002, (3): 49-52.
Citation: WEI Qi, LI Wen-jing, ZHU Xue-jun, HU Qiang. Study on Hardness and Redhardness of Surfacing Metal of Metal Powder-Cored Wire of Age Hardening Tool Alloy for TIG Surfacing[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2002, (3): 49-52.

时效硬化工具合金TIG金属粉芯焊丝堆焊金属硬度和红硬性

Study on Hardness and Redhardness of Surfacing Metal of Metal Powder-Cored Wire of Age Hardening Tool Alloy for TIG Surfacing

  • 摘要: 通过改变熔敷金属中Co元素的含量、焊后热处理工艺和堆焊层数,对时效硬化工具合金TIG金属粉芯焊丝堆焊金属的硬度、红硬性和时效硬化机理进行了研究。研究结果表明:Co元素含量和焊后热处理工艺对堆焊金属的硬度和红硬性有显著影响;当采用560℃×2.5h时效处理可使堆焊金属获得最佳时效效果;随Co含量增加,堆焊金属的硬度和红硬性增加,最高硬度可达70.2HRC,经650℃加热6h后的硬度仍能保持在60HRC以上。

     

    Abstract: By changing the content of cobalt and the technology of postheat treatment the following subjects are studied:the hardness and redhaitlness,the age hardening mechanism of the surfacing metal of metal powder-cored wire which is a type of age hardening tool alloy for TIC surfacing. The results of the study show that the effects of cobalt content and postheat treatment on hardness and redhaxdness are notable. With the increasing of cobalt content in deposited metal the hardness and redhardness of surfacing metal rise apparently. The hardness of surfacing metal can go up to HRC 69.4 and remain above HRC 60 after heated at 650℃ for 6 hours. The optimum age technology is 560℃×2.5 h.

     

/