高级检索
康继东, 耿雪霏. 非均质焊接接头裂纹尖端场的HRR主导性与J积分断裂判据[J]. 焊接学报, 1998, (3): 40-44.
引用本文: 康继东, 耿雪霏. 非均质焊接接头裂纹尖端场的HRR主导性与J积分断裂判据[J]. 焊接学报, 1998, (3): 40-44.
Kang Jidong, Geng Xuefei. HRR Dominance and J-integral as Fracture Parameter in Heterogeneous Welded Joint[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 1998, (3): 40-44.
Citation: Kang Jidong, Geng Xuefei. HRR Dominance and J-integral as Fracture Parameter in Heterogeneous Welded Joint[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 1998, (3): 40-44.

非均质焊接接头裂纹尖端场的HRR主导性与J积分断裂判据

HRR Dominance and J-integral as Fracture Parameter in Heterogeneous Welded Joint

  • 摘要: 采用反射式贴片云纹干涉法对焊接接头裂纹尖端位移场进行了测量,并考察了非均质焊接接头中的HRR主导有效性与J积分断裂判据的应用可行性。结果表明,至少对于本文所研究的情形而言,无论是A537钢采用LB52NS焊条施焊的高匹配接头,还是9% Ni钢,采用OK69.45焊条施焊的低匹配接头,横向位移场中HRR主导失效,而纵向位移场中lgv-lgr的线性关系不同于焊缝或母材的1/(n+1)。因此,在非均质焊接接头中直接应用J积分作为断裂判据不合适。同时,裂纹尖端采用奇异单元值得商榷。

     

    Abstract: HRR-dominace and the application feasibility of J-integral in heterogeneous welded joints is investigated by Moire interferometry of reflected sticking film.The results showed that at least for cases studied in this paper,for either the welded joint of steel A537 welded by electrode LB52NS with an overmatching weld in strength or the welded joint of steel 9% Ni welded by electrode OK69.45 with an undermatching weld in strength,HRR-dominance is failure in horizontal displacement field while the slope of lgv-lgr in vertical displacement field is not agreement with 1/(n+1) of base metal or weld metal.So,it is doubtful to directly use the J-integral as a fracture criterion in heterogeneous welded joints.By the way,it is also not correct to use sigularity elements in vinicity of the crack tip in welded joint.

     

/