再热裂纹新判据——(εr)min

New criterion of reheat cracking——(εr) min

  • 摘要: 采用等温插销试验,铁研试验和高温拉伸试验对HQ80C钢的再热裂纹敏感性进行了详尽的研究。用εpc的应变概念探讨了再热裂纹的形成条件,提出示意图,该图较完整地解释了影响再热裂纹各因素之间的关系。文中提出再热裂纹的新判据——(εr)min,讨论了判据的合理性和优点。研究结果表明:(εr)min愈小,材料的再热裂纹敏感性愈大。

     

    Abstract: The sensitivity of HQ80C steel to the reheat cracking was investigated by using the equi-temperature implant test,the Tekken test and the high-temperature tensile test.The conditions causing the reheat cracking were discussed utilizing the strain concept.Moreover,a scheme was proposed,which porfeotly discribes the relationship among the fectors affecting the reheat cracking.In this paper,the authors suggest a new oriterion of the reheat cracking——(εr) min,and desoribe its reasonableness and advantages.The less (εr) min is,the higher is the sensi-tivity of the materials to reheat cracking.

     

/