焊接振幅对铜/铝超声波焊接的影响

Effect of vibration amplitude on ultrasonic welding of Cu/Al

  • 摘要: 焊接振幅是超声波焊接的主要参数,但目前关于焊接振幅对超声波焊接影响机制的认识较少. 研究了焊接振幅对铜/铝超声波焊接过程,包括工件的振幅分配、界面温度、中间相分布、材料塑性变形以及接头性能的影响. 结果表明,在焊接压力1 575 N、焊接时间0.5 s时,随着焊接振幅增大,上工件振幅呈现近似线性增长;下工件振幅在焊接过程中均呈现逐渐近似线性增加的趋势. 在整个焊接过程中,焊接振幅越大,下工件的振幅越高. 在焊接振幅为25 μm时,获得了最大拉剪力为3150 N的铜/铝接头. 高的焊接振幅提升了焊头与上工件以及工件之间的相对运动速度,加速了焊接界面的温度升高及材料的塑性变形,增强了界面原子的扩散,最终促进了较高质量的铜/铝超声波焊接接头的形成.

     

    Abstract: Vibration amplitude is an important parameter of ultrasonic welding, but insights into the influence mechanism of vibration amplitude on ultrasonic welding are few. The effects of vibration amplitude on the process of Cu/Al ultrasonic welding were investigated in this study, including vibration amplitude distribution of specimens, interfacial temperature, intermediate phase distribution, materials plastic deformation, and properties of joint. The results show that under the welding pressure of 1575 N and welding time of 0.5 s, with the increase of welding amplitude, the vibration amplitudes of the upper specimen exhibit a linear growth, and the amplitudes of the lower specimen tend to show a near-linear growth. During the welding process, the higher the vibration amplitude, the higher the vibration amplitude of the lower specimen is. When the vibration amplitude is set at 25 μm, a Cu/Al joint is obtained with a maximum tensile-shear force of 3150 N. High vibration amplitude has increased the relative motion speed among the sonotrode, the upper specimen and the specimen, which has sped up the temperature rise in the welding interface and the plastic deformation of the material, thus accelerated the interfacial atoms diffusion and promoted the formation of high quality Cu/Al ultrasonic welding joints.

     

/