李帅贞, 邢艳双, 刘雪松. 转速对2060铝锂合金RFSSW接头成形及拉剪性能的影响[J]. 焊接学报, 2019, 40(10): 156-160. DOI: 10.12073/j.hjxb.2019400278
引用本文: 李帅贞, 邢艳双, 刘雪松. 转速对2060铝锂合金RFSSW接头成形及拉剪性能的影响[J]. 焊接学报, 2019, 40(10): 156-160. DOI: 10.12073/j.hjxb.2019400278
LI Shuaizhen, XING Yanshuang, LIU Xuesong. Effect of rotational speed on forming and tensile shear properties of 2060 Al-Li RFSSW joint[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2019, 40(10): 156-160. DOI: 10.12073/j.hjxb.2019400278
Citation: LI Shuaizhen, XING Yanshuang, LIU Xuesong. Effect of rotational speed on forming and tensile shear properties of 2060 Al-Li RFSSW joint[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2019, 40(10): 156-160. DOI: 10.12073/j.hjxb.2019400278

转速对2060铝锂合金RFSSW接头成形及拉剪性能的影响

Effect of rotational speed on forming and tensile shear properties of 2060 Al-Li RFSSW joint

  • 摘要: 以2060铝锂合金为研究对象,进行了回填式搅拌摩擦点焊试验,研究了不同转速下接头内部成形及其与拉伸性能的关系. 结果表明,点焊接头在不同转速下出现了未完全回填缺陷、孔洞缺陷及向下弯曲的钩状结构. 未完全回填缺陷与孔洞缺陷在低转速与高转速下易出现,钩状结构向下弯曲且随转速的增加其高度先增加再减小. 拉剪载荷随转速的提高先增加再降低;在转速为2 200 r/min时,接头拉剪载荷达到9 800 N. 拉剪试样的断裂方式均为剪切断裂,断裂位置可分为三类:沿搭接界面断裂、沿套筒作用区底部断裂及沿包含两者的混合断裂.

     

    Abstract: This study chose 2060 Al-Li alloy as the objective to perform RFSSW experiments. The purpose is to investigate the rotational speed on interior form and tensile shear properties of RFSSW joint. The results show that the incomplete refilled defect, void and hook occur in the RFSSW joints under different rotational speeds. Furthermore, the incomplete refilled defect and void easily occur at low and high rotational speeds. Meanwhile, hook bends toward downward and its height first increases and then reduces. The tensile shear load of joint increases and then decreases with increasing rotational speed. The maximum value reaches to 9 800 N under 2 200 r/min. The fracture mode of RFSSW joint is shear fracture, and the fracture location includes three types. They are along the lap interface, along the bottom of the sleeve affected zone and along the above-mentioned mixture fracture.

     

/