  • 摘要: 研制了以Fe-Ni-Mn-Si系为合金系的9Ni钢自保护药芯焊丝. 采用FCAW法在不加保护气体的条件下施焊,并对焊件进行了QLT(淬火+亚温淬火+回火)处理. 通过拉伸试验、低温冲击试验、金相分析、断口扫描等方法研究了焊接接头的力学性能、显微组织和断口形貌. 结果表明,所研制的药芯焊丝焊接接头抗拉强度为709 MPa,屈服强度为580 MPa,断后伸长率为26%,断面收缩率为47%. 力学性能满足9Ni钢的使用要求. 焊缝的组织为细晶铁素体+针状铁素体. QLT处理使焊缝的低温冲击吸收功从48 J/cm2提升至100 J/cm2,能够明显提高焊缝的低温韧性.

     

    Abstract: Self-shielded flux cored wire for 9%Ni steel with Fe-Ni-Mn-Si alloy system was developed. This wire was welded by FCAW with no shielding gas. QLT heat treatment was carried out after welding. Mechanical properties, microstructure, and fracture morphology of welded joint were studied by tensile testing, low temperature impact testing,metallurgical analysis, and SEM. The results show that, The tensile strength of welded joint is 709 MPa,the yield strength is 580 MPa, elongation ratio is 26%, section shrinkage rate is 47%. The mechanical properties meet the requirement of the use of 9%Ni steel. The microstructure of the weld metal consists of fine grain ferrite and acicular ferrite. QLT heat treatment increased low temperature impact energy of weld metal from 48 J/cm2 to 100 J/cm2. It can significantly improve the low temperature toughness of the weld.

     

/

返回文章
返回