Abstract:
Ni-base alloy and TiB
2/Ni-based alloy metal-ceramics coatings were obtained on low carbon steel surface by 5 kW CO
2 laser.Microstructure, phases, microhardness and sliding wear resistance of the coatings were studied.The results shown that Nibased alloy coating consists of γ-(Ni, Fe), Cr
23C
6 etc and TiB
2 Nibased alloy composite coating consists of γ-(Ni, Fe), Ni
3B, TiB
2 and TiC and so on.The Ni-based alloy coating is made up of flourishing γ-(Ni, Fe)dendrite and eutectic structure.Equiaxed solid solution and fine eutectic structure are observed in the TiB
2/Ni-based alloy composite coating.The influence of TiB
2 ceramics on microstructure of coating is prominent that the microstructure of coating is finer and the dendrite crystal gradually becomes equiaxed grain.The microhardness and wear resistance of Ni-based alloy can be improved remarkablely by adding TiB
2.