高级检索

八万吨模锻压机主缸焊接应力场有限元分析

陈重毅, 乔伟超, 麻永林, 邢淑清

陈重毅, 乔伟超, 麻永林, 邢淑清. 八万吨模锻压机主缸焊接应力场有限元分析[J]. 焊接学报, 2017, 38(5): 1-6. DOI: 10.12073/j.hjxb.20170501
引用本文: 陈重毅, 乔伟超, 麻永林, 邢淑清. 八万吨模锻压机主缸焊接应力场有限元分析[J]. 焊接学报, 2017, 38(5): 1-6. DOI: 10.12073/j.hjxb.20170501
CHEN Zhongyi, QIAO Weichao, MA Yonglin, XING Shuqing. Finite element analysis on master cylinder welding stress field of 80,000 tons of die forging press[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2017, 38(5): 1-6. DOI: 10.12073/j.hjxb.20170501
Citation: CHEN Zhongyi, QIAO Weichao, MA Yonglin, XING Shuqing. Finite element analysis on master cylinder welding stress field of 80,000 tons of die forging press[J]. TRANSACTIONS OF THE CHINA WELDING INSTITUTION, 2017, 38(5): 1-6. DOI: 10.12073/j.hjxb.20170501

八万吨模锻压机主缸焊接应力场有限元分析

基金项目: 国家科技重大专项资助项目(2009ZX04014-064-05);内蒙古自治区自然科学基金资助项目(2016MS0510)

Finite element analysis on master cylinder welding stress field of 80,000 tons of die forging press

  • 摘要: 针对八万吨模锻压机主缸焊接应力和变形难于精确控制的问题,建立了主缸焊接有限元模型,通过模拟计算和试验验证,得到了主缸焊接温度场、应力场和变形.结果表明,主缸焊接过程中焊缝温度最高,约为2 100℃,接头区域温度梯度最大.主缸焊后最大位移位于主缸顶部,位移量约为7.4 mm,焊缝区位移量较小.在焊接前应考虑对主缸底部和顶部进行约束,防止焊后产生较大变形.主缸焊缝区等效应力最大,约为470 MPa,热影响区应力次之,母材应力最小.在热处理前要注意接头上表面是否存在焊接裂纹等缺陷.以上结果为主缸实际焊接提供了计算数据参考.
    Abstract: In order to investigate welding stress distribution and deformation of master cylinder on 80 000 tons of die forging press, the master cylinder welding simulation model were built using finite element method, and the results of the master cylinder temperature field, stress and deformation were obtained. The results show that the maximum temperature of master cylinder is about 2 100 ℃, appearing in the weld area, and the maximum temperature gradient occurs in the joint area during the welding process. After the welding, the maximum displacement of the master cylinder is about 8 mm, located on top of the master cylinder, and the displacement amount of the weld zone is smaller compared to top of the master cylinder. In order to prevent large deformation and ensure assembly accuracy after welding, the displacement at top and bottom of the master cylinder must be constrained before welding. The maximum stress of master cylinder is about 470 MPa, appearing in the weld area, the stress in heat-affected zone is lower, which followed by the base metal zone. Before the heat treatment, it should be checked whether there are cracks on the surface of welding or other welding defects. These results can provide calculated data reference for actual production of the master cylinder.
  • [1] 张亦良, 崔栓伟, 李晓延. 液压支架主要承载构件焊接残余应力对比分析[J]. 焊接学报, 2013, 34(7): 89-92. Zhang Yiliang, Cui Shuanwei, Li Xiaoyan. Comparative analysis of residual stress of main components of hydraulic support[J]. Transactions of the China Welding Institution, 2013, 34(7): 89-92.
    [2] Dai H, Francis J A, Withers P J. Prediction of residual stress distributions for single weld beads deposited on to SA508 steel including phase transformation effects[J]. Materials Science and Technology, 2010, 26(8): 940-949.
    [3] 赵东升, 刘玉君, 孙敏科, 等. 碳钢与304不锈钢焊接残余应力的计算[J]. 焊接学报, 2012, 33(1): 93-95. Zhao Dongsheng, Liu Yujun, Sun Mingke, et al. Welding residual stress calculation of carbon steel and stainless steel joint[J]. Transactions of the China Welding Institution, 2012, 33(1): 93-95.
    [4] 杜 兵, 孙凤莲, 李小宇, 等. 试样尺寸对SA508-3钢焊接接头断裂韧度的影响[J]. 焊接学报, 2012, 33(6): 1-4. Du Bing, Sun Fenglian, Li Xiaoyu, et al. Effect of sample welded joint size on fracture toughness of SA508-3 steel[J]. Transactions of the China Welding Institution, 2012, 33(6): 1-4.
    [5] 郭咏华, 张贵锋, 杨宗奇, 等. Q690C低碳粒贝钢多层MAG焊接头组织与性能[J]. 焊接学报, 2015, 36(1): 96-100. Guo Yonghua, Zhang Guifeng, Yang Zongqi, et al. Microstructure and mechanical property of Q690C HSLA steel joint welded by meltipass metal active gas (MAG) welding process[J]. Transactions of the China Welding Institution, 2015, 36(1): 96-100.
    [6] Mark A F, Francis J A, Dai H, et al. On the evolution of local material properties and residual stress in a three-pass SA508 steel weld[J]. Acta Material, 2012, 60(8): 3268-3278.
    [7] 杜宝帅, 马学周, 张忠文, 等. 超细晶Q460钢多层多道焊接头残余应力的数值模拟[J]. 焊接学报, 2014, 35(2): 42-46. Du Baoshuai, Ma Xuezhou, Zhang Zhongwen, et al. Numerical simulation of residual stress in multipass weld joint of ultrafine-grained Q460 steel[J]. Transactions of the China Welding Institution, 2012, 35(2): 42-46.
    [8] 迟露鑫, 麻永林, 邢淑清, 等. 核电SA508-3钢厚壁圆筒纵向焊接残余应力分析[J]. 焊接学报, 2012, 33(6): 59-62. Chi Luxin, Ma Yonglin, Xing Shuqing, et al. Numerical simulation and experiments test of residual stress of longitudinal weld of thick SA508-3 steel pipe for nuclear power[J]. Transactions of the China Welding Institution, 2012, 33(6): 59-62.
    [9] 董俊慧, 霍立兴, 张玉凤. 环焊缝管道焊接应力应变三维有限元分析[J]. 机械工程学报, 2001, 37(12): 86-90. Dong Junhui, Huo Lixing, Zhang Yufeng. Three-dimensional finite element analysis of welding stress-strain in a girth welding pipe[J]. Chinese Journal of Mechanical Engineering, 2001, 37(12): 86-90.
    [10] 迟露鑫, 麻永林, 邢淑清, 等. 压力容器用钢板焊接温度场模拟与验证[J]. 焊接学报, 2012, 33(5): 61-64. Chi Luxin, Ma Yonglin, Xing Shuqingr, et al. Test verifies and simulation on welding steel plate for pressure vessel[J]. Transactions of the China Welding Institution, 2012, 33(5):61-64.
    [11] 迟露鑫, 麻永林. 核电SA508-3钢大型筒体环焊残余应力分析[J]. 焊接学报, 2013, 34(8): 85-88. Chi Luxin, Ma Yonglin. Analysis of residual stresses on large scale wall pipe weld of SA508-3 steel for nuclear power[J]. Transactions of the China Welding Institution, 2013, 34(8): 85-88.
  • 期刊类型引用(3)

    1. 迟大钊,郭涛,张闰琦,张涛,申浩. 声阻法胶接结构缺陷实时成像检测. 焊接学报. 2022(11): 107-111+168-169 . 本站查看
    2. 李家乐,王玉奇,李延辉,刘云韩,白硕玮,张鹏飞. 铝合金单搭胶接接头动态性能分析. 机械设计与研究. 2022(06): 86-89 . 百度学术
    3. 李永亮,黄涛,邸安乐. 填料改性对胶接应力影响的仿真研究. 中国胶粘剂. 2021(01): 29-32+52 . 百度学术

    其他类型引用(0)

计量
  • 文章访问数:  551
  • HTML全文浏览量:  5
  • PDF下载量:  513
  • 被引次数: 3
出版历程
  • 收稿日期:  2015-04-28

目录

    /

    返回文章
    返回